TI xLift Photoresist

TI xLift 
TI xLift is a image reversal photoresist for lift-off of thick films.

Film thickness:
4 ... 25 μm sales volumes: from 250 ml
UV-sensitivity:
i, h, and g-line (310 - 440 µm), broadband and monochromatic
Sales volumes: 250 ml, 500 ml, 1.000 ml, 2500 ml and 5 Liter

General Information

TI xLift is specially designed for the application in the so called "image reversal technology" for subsequent lift-off of thick and very thick deposited layers. For harsh chemical attack, such as direct mesa grooving in HF-HNO3 containing media or etching in high HF-concentrations prefer TI 35E.

What 'adjustable undercut means' - two examples

 
For further information refer Photoresist MicroChemicals TI xLift

 

  

 
®AZ, the AZ logo, BARLi , Aquatar and Kallista are registered trademarks of AZ Electronic Materials.

Overview
Sales volumes

Positive Thin
AZ® 111 XFS 
AZ® 1505 
AZ® 1512HS 
AZ® 1514H 
AZ® 1518 
AZ® 6612 
AZ® 6624 
AZ® 6632
AZ® MiR 701
AZ® ECI 3027

Positive Thick 
AZ® 4533
AZ® 4562 
AZ® 9260 
AZ® 40XT
 

Negative 
AZ®nLof 2070
AZ® 15nXT 
AZ® 125nXT 

Image Reversal/Lift-off
AZ® 5214E 
TI 35E 
TI 35ES 
TI Plating 
TI xLift  
AZ®nLof 2070
 

Deep-UV Photo Resist
AZ® TX 1311
 

Other Resists
AZ® 520D 
AZ®4999 
TI Spray 
PL 177 
AZ®Aquatar
AZ®Barli II

Other Resist Types  
Electroplating Resists
e-Beam Resists
Protective Coating

Spray Coating Resist
P. Circuit Board Resist
Antireflective Coating

Product Data Sheets
Safety Data Sheets
Brochure 2012
Application Notes

Tech Support Form
Interactive Support
Litho-Forum

New Products
New Documents
Exhibitions
Questionnaire

History 
Our Team
Field of Business
Quality Management
What else We Do
Imprint

 

© MicroChemicals 2011 Imprint